1.1 This specification covers the procedure for Charpy V-notch testing of structural steel and contains two frequencies of testing. The impact properties of steel can vary within the same heat and piece, be it as-rolled, control-rolled, or heat treated. The purchaser should, therefore, be aware that testing of one plate, bar, or shape does not provide assurance all plates, bars, or shapes of the same heat as processed will be identical in toughness with the product tested. Normalizing or quenching and tempering the product will reduce the degree of variation.
Author | ASTM |
---|---|
Editor | ASTM |
Document type | Standard |
Format | File |
ICS | 77.140.10 : Heat -treatable steels
|
Number of pages | 5 |
Replace | ASTM A673/A673M-07(2012) |
Set | ASTMVOL0104 |
Year | 2017 |
Document history | ASTM A673/A673M-07(2012) |
Country | USA |
Keyword | ASTM 673;ASTM A673;ASTM A673;10.1520/A0673_A0673M-17 |